Utilizing promoted Fe / rGO catalysts for the Fischer - Tropsch reaction in Slurry and Fixed Beds and studying their performance and Olefin productivity : A Thesis Submitted to the Graduate School of Innovative Design Engineering : Egypt - Japan University of Science and Technology (E - JUST) : In Partial Fulfillment of the Requirements for the Degree of Doctor of Philosophy in Material Science and Engineering / by AL-Hassan Mohammed Fawzy Nasser

By: Material type: TextTextLanguage: English Summary language: Arabic Publication details: Alexandria : AL-Hassan Mohammed Fawzy Nasser 2019Description: leaves 111 ; 30 cmOther title:
  • استخدام محفزات الحديد المنشطة و المحملة على أكسيد الجرافين المختزل في تفاعل فيشر - تروبش في مفاعلات المهد الثابت و المهد الطيني و دراسة أدائها ، و إنتاجيتها للأوليفينات / مقدمة من الحسن محمد فوزي ناصر للحصول على درجة (دكتوراه الفلسفة) في علم و هندسة المواد [Added title page title]
Issued also as a digital file (for more information please check our Digital Repository)Dissertation note: Thesis (Ph.D.) Doctoral Egypt - Japan University of Science and Technology (E-JUST) - School of Innovative Design Engineering - Material Science and Engineering Department 2019 Summary: هذه الرسالة تسلط الضوء على استخدام جزيئات الحديد النانومترية المحملة على صفائح أكسيد الجرافين المختزل كمادة حفازة لتفاعل فيشر - تروبش لتخليق مركبات الكربون المهدرج (الهيدروكاربونات) و في الجزء الأول من الاستقراء العملي تم إجراء التجارب الأولية (الاستكشافية) في مفاعل المهد المثبت المتوفر لدينا في معامل قسم علم و هندسة المواد في الجامعة المصرية اليابانية و في هذه المرحلة تم اختبار مواد الحديد / أكسيد الجرافين المختزل المحفزة الغير منشطة و المنشطة بعناصر البوتاسيوم و المنجنيز أعطت التجارب نسبة تحول لغاز أول أكسيد الكربون عالية جدا وصلت في أحسن الحالات لـ 96% مع المحفز المنشط بالبوتاسيوم و كانت أعلى معدلات الاختيارية نحو مركبات الهايدروكاربون الثقيلة 25% و تحققت أيضا مع المحفز المنشط بالبوتاسيوم و كونت التجارب المبدئية هذه الأساس العلمي و الخبرة العملية الأساسية لاستكمال الأبحاث في الجزء الثاني من الدراسة أجريت الاختبارات في معمل الأستاذ الدكتور / نوريتانسو تسوباكي في قسم الكيمياء التطبيقية في جامعة توياما باليابان و أجريت هناك دراسة تفصيلية لتأثير المنجنيز كعنصر منشط لمحفزات الحديد / أكسيد الجرافين المختزل عند تركيزات منجنيز و ظروف تشغيل مختلفة و لكن باستخدام مفاعل المهد الطيني المتوفر في معامل أ . د / تسوباكي و تركزت الدراسة حول تأثير منشط المنجنيز على إختيارية إنتاج الهيدروكربونات الغير مشبعة (الأوليفينات) و أظهرت التجارب أن مستوى التحميل المثالي للمنجنيز كمنشط للحديد / أكسيد الجرافين المختزل هو 0.16 مول منجنيز لكل مول حديد (Fen16) هذه النسبة تنتج الأوليفينات باختيارية تصل إلى 19% عند الظروف المثالية و كان تأثير المنجنيز بالسلب على نسبة تحول أول اكسيد الكربون فانخفضت إلى 62% عند التركيز المثالي للمنجنيز بعد أن كانت 83% قبل إضافة أي منشطات و كانت ظروف التشغيل المثالية لإنتاج الأوليفينات باختيارية 19% و نسبة أوليفين لبرافين 0.7 باستخدام المحفز FeMn16 هي 2MPa و حرارة 300°C و معدل سريان 4.2gh ضغط تم اختبار نفس محفزات الحديد منجنيز في مفاعل المهد الثابت و أنتجت الأوليفينات بأعلى معدلات انتاجية باستخدام FeMn29 عند ضغط 2MPa و حرارة 0°C23 و معدل سريان 4.2gh و بإنتاجية تصل إلى 34.5% كان المنتج في هذه الحالة غني بالأوليفينات الثقيلة أكثر من الخفيفة بينما لو استخدم نفس المحفز عند 340°C فإنه يعطي إنتاجية مقاربة 31.3% و لكن المنتج يكون أغنى بالأوليفينات الخفيفة عن الثقيلة تعمل منشطات المنجنيز على تنشيط الحديد خلال التفاعل عن طريق تكوين قشرة خارجية غنية بالمنجنيز حول المركز الغني بالحديد هذه القشرة تنظم دخول المتفاعلات للمركز الحديدي و تسرع من الامتزاز التحليلي لأول أكسيد الكربون بينما تقاوم الامتزاز التحليلي للهيدروجين هذا التأثير يزيد من درجة عدم التشبع في المنتج و يزيد من احتمالية نمو السلسلة مما يعطي منتجات أثقل و أغنى في الأوليفينات لم يظهر النحاس تحسن ملحوظ في النشاط عند استخدامه في المهد الطيني و رفع إنتاجية الأولفينات إلى 14% فقط بينما أعطى النحاس نشاط أعلى للمحفزات التي استخدم معها في مفاعلات المهد الثابت و نشط تفاعلات الهدرجة بينما بطأ من
Tags from this library: No tags from this library for this title. Log in to add tags.
Star ratings
    Average rating: 0.0 (0 votes)
Holdings
Item type Current library Call number Copy number Status Barcode
Dissertations Dissertations Fayza Aboulnaga Central Library | مكتبة فايزة أبو النجا المركزية بالحرم الجامعي MSE PhD. 2019 01 (Browse shelf(Opens below)) C. 1 Not for loan 10014974
Browsing Fayza Aboulnaga Central Library | مكتبة فايزة أبو النجا المركزية بالحرم الجامعي shelves Close shelf browser (Hides shelf browser)
MSE PhD. 2017 02 Development of High Performance Graphene Based Photocatalysts for Organic Synthesis and Energy Applications : A Thesis Submitted to the Graduate School of Innovative Design Engineering : Egypt - Japan University of Science and Technology (E - JUST) : In Partial Fulfillment of the Requirements for the Degree of Doctor of Philosophy in Material Science and Engineering / MSE PhD. 2017 03 Mechanic of Self - Healing Composites Based on Microcapsules : A Thesis Submitted to the Graduate School of Innovative Design Engineering : Egypt - Japan University of Science and Technology (E - JUST) : In Partial Fulfillment of the Requirements for the Degree of Doctor of Philosophy in Material Science and Engineering / MSE PhD. 2018 01 Study the Workability and Mechanical Properties of Binary B - type Ti - Alloys : A Thesis Submitted to the Graduate School of Innovative Design Engineering : Egypt - Japan University of Science and Technology (E - JUST) : In Partial Fulfillment of the Requirements for the Degree of Doctor of Philosophy in Material Science and Engineering / MSE PhD. 2019 01 Utilizing promoted Fe / rGO catalysts for the Fischer - Tropsch reaction in Slurry and Fixed Beds and studying their performance and Olefin productivity : A Thesis Submitted to the Graduate School of Innovative Design Engineering : Egypt - Japan University of Science and Technology (E - JUST) : In Partial Fulfillment of the Requirements for the Degree of Doctor of Philosophy in Material Science and Engineering / MSE PhD. 2019 02 Study of Ternary Rubber Blend Composites for Engineering Applications : A Thesis Submitted to the Graduate School of Innovative Design Engineering : Egypt - Japan University of Science and Technology (E - JUST) : In Partial Fulfillment of the Requirements for the Degree of Doctor of Philosophy in Material Science and Engineering / MSE PhD. 2019 03 Design and Characterization of Low - Cost High Entropy Alloys with High Strength : A Thesis Submitted to the Graduate School of Innovative Design Engineering : Egypt - Japan University of Science and Technology (E - JUST) : In Partial Fulfillment of the Requirements for the Degree of Doctor of Philosophy in Material Science and Engineering / MSE PhD. 2020 01 Deformation Characteristics of Tiny Aluminum Pins Fabricated by Cold Extrusion Process in Micro / Meso - Scale : A Thesis Submitted to the Graduate School of Innovative Design Engineering : Egypt - Japan University of Science and Technology (E - JUST) : In Partial Fulfillment of the Requirements for the Degree of Doctor of Philosophy in Material Science and Engineering /

Includes a title page in Arabic

Thesis (Ph.D.) Doctoral Egypt - Japan University of Science and Technology (E-JUST) - School of Innovative Design Engineering - Material Science and Engineering Department 2019

هذه الرسالة تسلط الضوء على استخدام جزيئات الحديد النانومترية المحملة على صفائح أكسيد الجرافين المختزل كمادة حفازة لتفاعل فيشر - تروبش لتخليق مركبات الكربون المهدرج (الهيدروكاربونات) و في الجزء الأول من الاستقراء العملي تم إجراء التجارب الأولية (الاستكشافية) في مفاعل المهد المثبت المتوفر لدينا في معامل قسم علم و هندسة المواد في الجامعة المصرية اليابانية و في هذه المرحلة تم اختبار مواد الحديد / أكسيد الجرافين المختزل المحفزة الغير منشطة و المنشطة بعناصر البوتاسيوم و المنجنيز أعطت التجارب نسبة تحول لغاز أول أكسيد الكربون عالية جدا وصلت في أحسن الحالات لـ 96% مع المحفز المنشط بالبوتاسيوم و كانت أعلى معدلات الاختيارية نحو مركبات الهايدروكاربون الثقيلة 25% و تحققت أيضا مع المحفز المنشط بالبوتاسيوم و كونت التجارب المبدئية هذه الأساس العلمي و الخبرة العملية الأساسية لاستكمال الأبحاث في الجزء الثاني من الدراسة أجريت الاختبارات في معمل الأستاذ الدكتور / نوريتانسو تسوباكي في قسم الكيمياء التطبيقية في جامعة توياما باليابان و أجريت هناك دراسة تفصيلية لتأثير المنجنيز كعنصر منشط لمحفزات الحديد / أكسيد الجرافين المختزل عند تركيزات منجنيز و ظروف تشغيل مختلفة و لكن باستخدام مفاعل المهد الطيني المتوفر في معامل أ . د / تسوباكي و تركزت الدراسة حول تأثير منشط المنجنيز على إختيارية إنتاج الهيدروكربونات الغير مشبعة (الأوليفينات) و أظهرت التجارب أن مستوى التحميل المثالي للمنجنيز كمنشط للحديد / أكسيد الجرافين المختزل هو 0.16 مول منجنيز لكل مول حديد (Fen16) هذه النسبة تنتج الأوليفينات باختيارية تصل إلى 19% عند الظروف المثالية و كان تأثير المنجنيز بالسلب على نسبة تحول أول اكسيد الكربون فانخفضت إلى 62% عند التركيز المثالي للمنجنيز بعد أن كانت 83% قبل إضافة أي منشطات و كانت ظروف التشغيل المثالية لإنتاج الأوليفينات باختيارية 19% و نسبة أوليفين لبرافين 0.7 باستخدام المحفز FeMn16 هي 2MPa و حرارة 300°C و معدل سريان 4.2gh ضغط تم اختبار نفس محفزات الحديد منجنيز في مفاعل المهد الثابت و أنتجت الأوليفينات بأعلى معدلات انتاجية باستخدام FeMn29 عند ضغط 2MPa و حرارة 0°C23 و معدل سريان 4.2gh و بإنتاجية تصل إلى 34.5% كان المنتج في هذه الحالة غني بالأوليفينات الثقيلة أكثر من الخفيفة بينما لو استخدم نفس المحفز عند 340°C فإنه يعطي إنتاجية مقاربة 31.3% و لكن المنتج يكون أغنى بالأوليفينات الخفيفة عن الثقيلة تعمل منشطات المنجنيز على تنشيط الحديد خلال التفاعل عن طريق تكوين قشرة خارجية غنية بالمنجنيز حول المركز الغني بالحديد هذه القشرة تنظم دخول المتفاعلات للمركز الحديدي و تسرع من الامتزاز التحليلي لأول أكسيد الكربون بينما تقاوم الامتزاز التحليلي للهيدروجين هذا التأثير يزيد من درجة عدم التشبع في المنتج و يزيد من احتمالية نمو السلسلة مما يعطي منتجات أثقل و أغنى في الأوليفينات لم يظهر النحاس تحسن ملحوظ في النشاط عند استخدامه في المهد الطيني و رفع إنتاجية الأولفينات إلى 14% فقط بينما أعطى النحاس نشاط أعلى للمحفزات التي استخدم معها في مفاعلات المهد الثابت و نشط تفاعلات الهدرجة بينما بطأ من

Issued also as a digital file (for more information please check our Digital Repository)

(IDE) School of Innovative Design Engineering (MSE) Materials Science Engineering

There are no comments on this title.

to post a comment.

Click on an image to view it in the image viewer

Local cover image

All Rights Reserved
Egypt-Japan University of Science and Technology (E-JUST) © 2024